Min Temp
Max Temp
🌡
⚡
🛡
⚖
Product Overview
Nimonic 80A threaded rods are high-strength nickel-chromium alloy fasteners manufactured from UNS N07080 bar stock, conforming to ASTM B637. This precipitation-hardened alloy is strengthened by additions of titanium and aluminium, providing exceptional creep and oxidation resistance up to 815°C. Nimonic 80A threaded rods are widely specified for bolted joints in high-temperature environments where standard stainless steels fail due to thermal relaxation or scaling.
These rods are commonly used in gas turbine engines, exhaust manifolds, and petrochemical furnace assemblies, where their ability to maintain mechanical integrity under cyclic thermal loads is critical. All Nimonic 80A threaded rods are supplied with full traceability and certification to international standards.
| Material | Nimonic 80A |
| UNS Number | N07080 |
| DIN Number | 2.4952 / 2.4631 |
| Material Standard | ASTM B637 |
| Rod Standard (Metric) | DIN 975 / DIN 976 |
| Rod Standard (Inch) | ASME B18.31.3 |
| Thread Form | ISO Metric / UNC / UNF |
| Diameter Range | M6-M48 / ¼"-2" |
| Tensile Strength | 950 MPa (138 ksi) min |
| Yield Strength | 690 MPa (100 ksi) min |
| Hardness | Max 35 HRC / 320 HB |
Complete the Fastener Set
Technical Data
| Size (M) | Pitch (mm) | Rod Dia (mm) | Standard Length (mm) | Custom Length (mm) |
|---|---|---|---|---|
| M6 | 1.0 | 6.0 | 1000 | 100-2000 |
| M8 | 1.25 | 8.0 | 1000 | 100-2000 |
| M10 | 1.5 | 10.0 | 1000 | 100-2000 |
| M12 | 1.75 | 12.0 | 1000 | 100-2000 |
| M16 | 2.0 | 16.0 | 1000 | 100-2000 |
| M20 | 2.5 | 20.0 | 1000 | 100-2000 |
| M24 | 3.0 | 24.0 | 1000 | 100-2000 |
| M30 | 3.5 | 30.0 | 1000 | 100-2000 |
| M36 | 4.0 | 36.0 | 1000 | 100-2000 |
| M42 | 4.5 | 42.0 | 1000 | 100-2000 |
| M48 | 5.0 | 48.0 | 1000 | 100-2000 |
| Standard | Covers | Thread |
|---|---|---|
| DIN 975 | Threaded rods, full thread | Metric |
| DIN 976 | Stud bolts, double end | Metric |
| ASME B18.31.3 | Threaded rods | UNC/UNF |
| ISO 898-1 | Mechanical properties | Metric |
| Material Standard | Requirement |
|---|---|
| ASTM B637 | Bar/rod - UNS N07080 |
| BS HR1 | Rod/Bar - Nimonic 80A |
| AMS 5829 | High-temp fasteners |
| EN 10204 3.1 | Mill test certificate |
| EN 10204 3.2 | TPI-witnessed MTC |
Material Chemistry
| Element | Composition (%) |
|---|---|
| Nickel (Ni) | 69.0 min |
| Chromium (Cr) | 18.0-21.0 |
| Cobalt (Co) | 2.0 max |
| Titanium (Ti) | 1.8-2.7 |
| Aluminium (Al) | 1.0-1.8 |
| Carbon (C) | 0.10 max |
| Iron (Fe) | 3.0 max |
| Manganese (Mn) | 1.0 max |
| Silicon (Si) | 1.0 max |
| Copper (Cu) | 0.2 max |
| Zirconium (Zr) | 0.15 max |
| Boron (B) | 0.006 max |
| Sulphur (S) | 0.015 max |
Fastener Performance
| Rod Size | Dry (Nm) | Lubricated (Nm) | Clamp Load (kN) |
|---|---|---|---|
| M12 | 110 | 88 | 38 |
| M16 | 260 | 208 | 85 |
| M20 | 520 | 416 | 136 |
| M24 | 900 | 720 | 200 |
| M30 | 1800 | 1440 | 320 |
| M36 | 3100 | 2480 | 470 |
| M42 | 5000 | 4000 | 650 |
| M48 | 7400 | 5920 | 900 |
Industry Applications